The aim of this work was to combine the properties of chlorobutyl rubber (CIIR) and natural rubber (NR) in a binary blend for application in the inner liner of tubeless tires, using organomodified montmorillonite (Cloisite® 15A) as filler in order to improve the barrier property of the material. The maintenance of the mechanical and barrier properties of CIIR/NR 60/40 indicated that this blend can be used in the inner liner of tubeless tires, thereby reducing the cost of the final product, since the CIIR is 80% more expensive than NR.
RattanasomNPrasertsriS. Relationship among mechanical properties, heat ageing resistance, cut growth behaviour and morphology in natural rubber: partial replacement of clay with various types of carbon black at similar hardness level. Polym Test2009; 28: 270–276.
Sinha RaySOkamotoM. Polymer/layered silicate nanocomposites: a review from preparation to processing. Prog Polym Sci2003; 28: 1539–1641.
10.
ChoudalakisGGotsisAD. Permeability of polymer/clay nanocomposites: a review. Eur Polym J2009; 45: 967–984.
11.
MaiY-WYuZ-Z. Polymer nanocomposites. Boca Raton: CRC Press, 2006, pp. 273–296.
12.
ASTM D1646:2003. Standard test methods for rubber-viscosity stress relaxation and pre-vulcanization characteristics (Mooney Viscometer).
13.
ASTM D2084:2006. Standard test method for rubber property-Vulcanization using oscillating disk meter.
14.
ASTM D3418:2008. Standard test methods for transition temperatures and enthalpies of fusion and crystallization of polymers by differential scanning calorimetry.
15.
ASTM D624:2000. Standard test method for tear strength of conventional vulcanized rubber and thermoplastic elastomers.
16.
ASTM D412:2006. Standard test methods for vulcanized rubber and thermoplastic elastomers-Tension.
17.
ASTM D3182:2007. Standard for rubber: materials, equipment, and procedures for mixing standard compounds and preparing standard vulcanized sheets.
18.
ASTM D2240:2005. Standard test method for rubber property-Durometer hardness.
19.
ASTM D1927:2007. Standard test methods for determination of oxygen gas transmission rate, permeability and permeance at controlled relative humidity through barrier materials using a coulometric detector.
CarliLNRoncatoCRZanchetA. Characterization of natural rubber nanocomposites filled with organoclay as a substitute for silica obtained by the conventional two-roll mill method. Appl Clay Sci2011; 52: 56–61.
22.
SapkotaJPoikelispääMDasA. Influence of nanoclay-carbon black hybrid fillers on cure and properties of natural rubber compounds. Polym Eng Sci2013; 53: 615–622.
23.
López-ManchadoMAHerreroBArroyoM. Organoclay–natural rubber nanocomposites synthesized by mechanical and solution mixing methods. Polym Int2004; 53: 1766–1772.
24.
SepehriARazzaghi-KashaniMGhoreishyMHR. Vulcanization kinetics of butyl rubber–clay nanocomposites and its dependence on clay microstructure. J Appl Polym Sci2011; 125: E204–E213.
25.
MalasADasCK. Selective dispersion of different organoclays in styrene butadiene rubber in the presence of a compatibilizer. Mater Des2013; 49: 857–865.
26.
López-ManchadoMAHerreroBArroyoM. Preparation and characterization of organoclay nanocomposites based on natural rubber. Polym Int2003; 52: 1070–1077.
27.
Carretero-GonzálezJValentínJLArroyoM. Natural rubber/clay nanocomposites: influence of poly(ethylene glycol) on the silicate dispersion and local chain order of rubber network. Eur Polym J2008; 44: 3493–3500.
28.
DasACostaFRWagenknechtU. Nanocomposites based on chloroprene rubber: effect of chemical nature and organic modification of nanoclay on the vulcanizate properties. Eur Polym J2008; 44: 3456–3465.
29.
RajasekarRNayakGCMalasA. Development of compatibilized SBR and EPR nanocomposites containing dual filler system. Mater Des2012; 35: 878–885.
30.
QuLHuangGZhangP. Synergistic reinforcement of nanoclay and carbon black in natural rubber. Polym Int2010; 59: 1397–1402.
31.
OkamotoMMoritaSTaguchiH. Synthesis and structure of smectic clay/poly(methyl methacrylate) and clay/polystyrene nanocomposites via in situ intercalative polymerization. Polymer2000; 41: 3887–3890.
32.
VaiaRAGiannelisEP. Polymer melt intercalation in organically-modified layered silicates: model predictions and experiment. Macromolecules1997; 30: 8000–8009.
33.
MaitiMSadhuSBhowmickAK. Effect of carbon black on properties of rubber nanocomposites. J Appl Polym Sci2005; 96: 443–451.
34.
GalALYangXKluppelM. Evaluation of sliding friction and contact mechanics of elastomers based on dynamic-mechanical analysis. J Chem Phys2005; 123: 014704.
35.
PraveenSChattopadhyayPKAlbertP. Synergistic effect of carbon black and nanoclay fillers in styrene butadiene rubber matrix: development of dual structure. Compos A Appl Sci Manuf2009; 40: 309–316.
36.
LiuYLiLWangQ. Effect of carbon black/nanoclay hybrid filler on the dynamic properties of natural rubber vulcanizates. J Appl Polym Sci2010; 118: 1111–1120.
37.
YehiaAAAkelahAMRehabA. Evaluation of clay hybrid nanocomposites of different chain length as reinforcing agent for natural and synthetic rubbers. Mater Des2012; 33: 11–19.
38.
RattanasomNPrasertsriSRuangritnumchaiT. Comparison of the mechanical properties at similar hardness level of natural rubber filled with various reinforcing-fillers. Polym Test2009; 28: 8–12.
39.
SridharVShanmugharajAMKimJK. Optimization of carbon black nanoclay filler loading in chlorobutyl vulcanizates using response surface methodology. Polym Compos2009; 30: 691–701.