The anisotropy of mechanical properties in the context of steels used to fabricate large diameter pipes can be detrimental to the design and performance of the pipes. We examine here the anisotropy of strength and toughness, and with the help of detailed characterisation show that there is a complex interaction between the ability of the steel to delaminate on the rolling plane and the crystallographic texture, which promotes brittle fracture on the macroscopic fracture plane of Charpy specimens.
SeoD. H., KimC. M., YooJ. Y. and KangK. B.:Proc. 17th Int. Offshore and Polar Engineering Conf., Lisbon, Portugal, July 2007, The International Society of Offshore and Polar Engineers, 3301–3306.
2.
StalheimD., BarnesK. and McCutcheonD.:‘Microalloyed steels for the oil and gas industry’, 73–108; 2007, Warrendale, PA, TMS.
KimK. and BaeJ.-H.:Proc. 7th Int. Pipeline Conf., Calgary, Alta., Canada, October 2008, ASME, Vol. 3, 167–173.
5.
SimsC. E.:Trans. Metall. Soc. AIME, 1959, 215, 367–393.
6.
HodgeJ. M., FrazierR. H. and BoulgerF. W.:Trans. Metall. Soc. AIME, 1959, 215, 745–753.
7.
BakerT. J. and CharlesJ. A.:J. Iron Steel Inst., 1972, 210, 680–690.
8.
WilsonP. C., MurtyY. V., KattamisT. Z. and MehrabianR.:Met. Technol., 1975, 2, 241–244.
9.
MatrosovY. I. and PolyakovI. E.;Stal, 1976, 2, 162–167.
10.
GarwoodS. J.:in‘Application of fracture mechanics to materials and structures’, 939–950; 1984, Leiden, Martinus Nijhoff Publishers.
11.
KramerG. S., WilkowskiG. M. and MaxeyW. A.:‘Flaw tolerance of spiral–welded line pipe’, Technical report no. L51514, American Gas Association, Washington, DC, USA, 1987.
12.
BurnosV. A., VaschiloT. P. and BalandinaL. E.:Ind. Lab. (USSR), 1988, 54, 548–550.
13.
WilkowskiG. M., AhmadJ., BrustF., GhadialiN., KrishnaswamyP., LandowM., MarschallC. W., ScottP. and ViethP.:‘Short cracks in piping and piping welds’, Technical report no. NUREG/CR-4599-Vol. 1-No. 1; BMI–2173-Vol. 1-No. 1, Nuclear Regulatory Commission, Columbus, Ohio, USA, 1991.
14.
KrishnaswamyP., ScottP., MohanR., RahmanS., ChoiY. H., BrustF., KilnskiT., GhadialiN., MarchallC. and WilkowskiG.:‘Fracture behavior of short circumferentially surface-cracked pipe’, Technical report np. NUREG/CR-6298, Nuclear Regulatory Commission, Columbus, Ohio, USA, 1995.
15.
MintzB., MorrisonW. B., WelchP. I. and DaviesG. J.:in‘Texture of materials’, (ed. GottsteinG. and LuckeK.), Vol. 2, 465–474; 1978, Berlin, Springer-Verlag.
16.
InagakiH., KuriharaK. and KozasuI.:Trans. Iron Steel Inst. Jpn, 1977, 17, 75–81.
17.
BaczynskiG. J., JonasJ. J. and CollinsL. E.:Metall. Mater. Trans. A, 1999, 30A, 3045–3054.
18.
PetrovR. H., GarciaO. L., MuldersJ. J. L., ReisA. C. C., BaeJ. H., KestensL. A. I. and HoubaertY.:Mater. Sci. Forum, 2007, 550, 625–630.
19.
JuJ. B., LeeJ. S. and JangJ. I.:Mater. Lett., 2007, 61, 5178–5180.
20.
MintzB., MorrisonW. B., MorrisP. P. and DaviesG. J.:in‘Texture and properties of materials’, (ed. DaviesG. J.), 224–234; 1976, London, The Metals Society.
21.
FegredoD. M., FaucherB. and ShehataM. T.:‘Strength of metals and alloys’, Vol. 2, 1127–1132; 1985, Oxford, Pergamon Press.